Estudo do efeito de mudanças sucessivas na trajetória de deformação no comportamento mecânico dos aços inoxidáveis ferríticos AlSl 430 e AlSl 441
dc.contributor.advisor | Lopes, Wellington | |
dc.contributor.advisor-co | Corrêa, Elaine Carballo Siqueira | |
dc.contributor.advisor-coLattes | http://lattes.cnpq.br/3203046752707862 | |
dc.contributor.advisorLattes | http://lattes.cnpq.br/4445376135095677 | |
dc.contributor.author | Alencar, Rafael Alves Frederico de | |
dc.contributor.authorLattes | http://lattes.cnpq.br/1935110479565192 | |
dc.contributor.referee | Lopes, Wellington | |
dc.contributor.referee | Corrêa, Elaine Carballo Siqueira | |
dc.contributor.referee | Magalhães, Frederico de Castro | |
dc.contributor.referee | Aguilar, Maria Teresa Paulino | |
dc.date.accessioned | 2025-03-25T17:49:01Z | |
dc.date.available | 2025-03-25T17:49:01Z | |
dc.date.issued | 2016-04-05 | |
dc.description.abstract | Os aços inoxidáveis são, basicamente, ligas de ferro-cromo-carbono que devido à sua resistência à corrosão, ao impacto, à abrasão, à durabilidade e às suas propriedades estéticas, constituem um material atrativo para satisfazer diversos tipos de demanda. Porém, antes de possuírem as formas e dimensões finais para a sua utilização, todo material necessita ser processado, uma dessas etapas é a conformação mecânica. Ao submeter um material a esse processo ocorrem diversos fenômenos que alteram suas características mecânicas, os quais geralmente podem ser previstos. Porém em materiais que possuem orientações preferenciais e com trajetória de deformação alterada, torna-se mais difícil prever o respectivo comportamento mecânico após tais operações, podendo assim ocorrer o amaciamento ou o endurecimento, sendo os mesmos influenciados por diversas variáveis como as condições de aquecimento, a composição química do material, o tipo de esforço e a taxa de deformação aplicados ao material. Diante do exposto e considerando a dependência entre as condições de solicitação mecânica e as respostas exibidas pelos diferentes tipos de materiais, este projeto de pesquisa apresenta o estudo das respostas mecânicas em diferentes trajetórias de deformação para os aços inoxidáveis AISI 430 e AISI 441, na forma de chapas em carregamentos monotônicos e combinados. Os resultados indicaram que o comportamento mecânico dos aços inoxidáveis depende das condições de aplicação do esforço, em termos de direção, quantidade e combinação de esforços mecânicos. Foi observado ainda o amaciamento dos materiais pré-deformados em tração e o encruamento dos materiais por meio de uma operação de estampagem quando comparado com o carregamento sob cisalhamento no estado como recebido dos aços AISI 430 e AISI 441. | |
dc.description.abstractother | The ceramic materials fundamentally of poly-silico-aluminates (or geopollymeric), environmental polymerization, can be produced using as raw material several types of waste available in the industry, being very favorable to the environment, because they requires a very few energy for processing. In the case of concrete inorganic polymers (geopolymeric cement), the polymer paste still serve to bind the grown and small aggregates and / or any other non-reactive materials. This process of polymerization involves strongly alkaline reactions (NaOH), in the presence of minerals containing Al-Si, producing the polymeric binder of the type Si-O-Al-O allowing curing at room temperature. The production of ceramic materials is dependent on composition, process and desired applications. In this work, the main input used was porcelain, discarded of processing of sink and toilets, with aesthetic defects (DECA). These porcelains are composed by kaolinitic clay, quartz and feldspar. They pass through a burning process between 1.000º C and 1.300 °C (or 1.832º F and 2.372º F) for several hours, forming a glass phase in addition to alpha quartz, mullite primary and secondary. This will be an important factor in the reuse or recycling of porcelain, as it is the same, strongly influenced by the amount of glassy phase (inducing the pozzolanic reaction) and the presents crystalline phases. The sanitary porcelains production process also employs the gypsum in molds, having a certain lifetime is discarded thereafter. Currently, a big part of these two industrial waste going to landfills, or is thrown incorrectly as waste from construction and demolition (RCD). This work deals with the study reuse of this waste in order to obtain, produce and characterize paste from ceramic waste. It were used as raw materials (industrial waste): porcelain (about 50 to 70% by weight), gypsum as a handle reducer (10%), the ore dolomite as chamotte (0 or 10%), plus a binder alkali NaOH (10 to 20%) which, after the addition of manipulation water, were made test specimens (CPs). They were made physicochemical characterizations of CPs, mechanical and thermal analysis of materials obtained. The results of the mechanical and thermal tests were satisfactory, showed great possibility of using waste, as raw material, in the production of geopolymeric cements. With this procedure, we tried to give a useful waste destination, transforming them into a new product with higher added value, environmental and technological point of view. | |
dc.description.sponsorship | Coordenação de Aperfeiçoamento de Pessoal de Nível Médio (CAPES), Aperam South América. | |
dc.identifier.uri | https://repositorio.cefetmg.br//handle/123456789/936 | |
dc.language.iso | pt | |
dc.publisher | Centro Federal de Educação Tecnológica de Minas Gerais | |
dc.publisher.country | Brasil | |
dc.publisher.initials | CEFET-MG | |
dc.publisher.program | Programa de Pós-Graduação em Engenharia de Materiais | |
dc.subject | Comportamento mecânico | |
dc.subject | Cisalhamento (Ensaios) | |
dc.subject | Aço inoxidável ferrítico | |
dc.subject | Deformação plástica | |
dc.title | Estudo do efeito de mudanças sucessivas na trajetória de deformação no comportamento mecânico dos aços inoxidáveis ferríticos AlSl 430 e AlSl 441 | |
dc.type | Dissertação |
Arquivos
Pacote Original
1 - 1 de 1
Carregando...
- Nome:
- Estudo do efeito de mudanças sucessivas na trajetória de deformação no comportamento mecânico dos aços inoxidáveis ferríticos AlSl 430 e AlSl 441.pdf
- Tamanho:
- 3.72 MB
- Formato:
- Adobe Portable Document Format
Licença do Pacote
1 - 1 de 1
Nenhuma Miniatura disponível
- Nome:
- license.txt
- Tamanho:
- 1.39 KB
- Formato:
- Item-specific license agreed to upon submission
- Descrição: